Sludge dewatering: polymer, machine and cake solids

A wet cake is usually diagnosed as a polymer problem and fixed by buying more polymer. Most of the time it is a charge, drainage or machine-setting problem wearing a polymer costume.

Last updated: 2026-11-18Technical article

Quick answer: sludge dewatering is decided by three things in order — the sludge's charge demand, the polymer dose that matches it, and the machine's drainage and pressure settings. Raising the polymer dose without checking charge and machine settings usually produces a stickier cake, not a drier one.

Where the water actually is

Sludge water sits in three places: free water between flocs, interstitial water inside the floc structure, and bound water in the cell mass. Mechanical dewatering removes free and part of the interstitial water. Bound water needs thermal drying or chemical conditioning that changes the cell structure — no press removes it.

That is why cake solids have a practical ceiling: about 20–25% for waste-activated sludge on a belt press, 25–32% on a high-solids centrifuge, higher for digested or thermally conditioned sludge.

Charge demand before dose

Sludge particles are negatively charged; cationic polymer neutralises that charge and bridges the flocs. The correct dose is set by the charge, not by the tonnage.

Sludge typeCharge behaviourPractical note
Waste-activated, youngHigh negative chargeHigher charge density needed; dose is high
Waste-activated, oldLower charge, more dispersedLower density, watch for overdosing
DigestedLower charge, finer solidsMedium density, good drainage
Primary + secondary mixedVariableTest the actual mix, not the design mix
Chemical sludge (PAC/lime)Already coagulatedPolymer dose low; overdosing is easy

A charge-demand test — titrating with a standard polymer until the supernatant clears — takes ten minutes and typically explains a 30–50% dose difference between two plants with the same sludge volume.

Conditioning dose

  • Cationic PAM 0.2–1.5 kg per tonne of dry solids, with 0.5–1.0 kg/t as the common municipal range.
  • Prepare 0.1–0.2% stock, dilute to 0.05% at the injection point, and provide 30–60 seconds of gentle mixing before the machine.
  • Too little: free water remains, cake wet, filtrate turbid.
  • Too much: cake sticky, cloth blinds, solids climb in the filtrate, and the polymer bill rises with worse results.

The dose curve has a clear minimum: plot cake solids and filtrate solids against polymer dose, and the optimum is where filtrate clarity is acceptable and cake solids peak.

Machine settings

SettingEffectPractical starting point
Polymer doseFloc size and strengthFrom the jar/screen test, then trim on site
Conditioning timeFloc maturity30–60 s gentle mixing, not in a pump
Belt speedDrainage time and cake thicknessSlower for wet sludge, faster if cake is too dry and cracking
Belt tension / pressureCake solidsIncrease in steps, watch for crushing and cloth wear
Gravity drainage zoneFree water removalPloughs and deck condition matter more than pressure
Centrifuge bowl speed / differentialCake dryness vs torqueSmall differential changes have large effects

Diagnosing a wet cake

  1. Filtrate turbid, cake wet — underdose or wrong charge density.
  2. Filtrate clear, cake wet — drainage or pressure problem, not polymer.
  3. Cake sticky, cloth blinding — overdose or too high a charge density.
  4. Solids in filtrate climbing — floc sheared in the feed pump or the dose point is too far upstream.
  5. Performance falls after a sludge age change — re-run the charge test; do not simply raise the dose.

Data to send

  • Sludge type, DS%, VS%, and the machine type.
  • Current polymer, dose, cake solids and filtrate solids.
  • A 2–5 kg sample and the target cake solids.

That is enough to propose a grade and a dose band, and to say whether the target is physically reachable on the existing machine.

Questions buyers ask

Direct answers

Can polymer make cake solids much higher?

Within the machine's limit, yes; beyond it, no. Bound water and machine design set the ceiling. Polymer fixes a wet cake only when the cause is flocculation, not when it is drainage area or pressure.

Why does the centrifuge cake get wetter at higher throughput?

Residence time and differential speed drop, so drainage and compaction suffer. Trim the feed or the differential before adding polymer.

What dose should we start with?

0.5–1.0 kg/t DS for municipal mixed sludge, then trim on site. Charge-demand testing narrows it faster than a dose ladder alone.

Does polymer damage the downstream dryer?

Excess polymer can raise the stickiness of the cake and load the dryer. Keeping the dose near the optimum protects both the press and the dryer.

Send your water or material data.